Page 1 of 1
Tenacious scale and hardware mod
Posted: Tue Jan 04, 2011 6:21 pm
by jforbush
Posted: Tue Jan 04, 2011 6:28 pm
by feed_the_animals
Nice. Cerakote on the liners I imagine? What about the G-10? Thanks for sharing.
Posted: Tue Jan 04, 2011 6:30 pm
by jforbush
Cerakote on everything that is OD green.
Posted: Tue Jan 04, 2011 6:37 pm
by angusW
Great job jforbush. Love seeing mods on the Ten.
Posted: Tue Jan 04, 2011 7:10 pm
by feed_the_animals
I don't know much about Cerakote. If you don't mind my asking, doesn't it need to be baked? I know G10 is resistant to temp extremes so it must fall within cerakote's baking temp. What is the baking temp? tia
Posted: Tue Jan 04, 2011 8:25 pm
by Jay_Ev
That looks great! And is that a poop magnet patch? LOL
Posted: Tue Jan 04, 2011 8:35 pm
by jforbush
Why yes it is a sh@t magnet patch!! :)
Cerakote is a bake on finish. I lower the regular temp from 250 to 175 and bake for 2 hours. I can lower the temp more but I have found 175 to be more than enough to get the job done.
And thanks all for the compliments....constructive criticism is welcomed as well.
Posted: Tue Jan 04, 2011 10:09 pm
by Rev. Chuck
Where do I send mine and how much you would charge for something like that =]
Posted: Tue Jan 04, 2011 10:20 pm
by jforbush
I pm'ed you Rev.....just shoot me an email please.
Posted: Mon Feb 28, 2011 6:41 pm
by GRIFFIN HAWKS
Ha !
Posted: Mon Feb 28, 2011 7:45 pm
by tonydahose
looks nice
Posted: Mon Feb 28, 2011 8:09 pm
by WhitefeatherTexas
Sweet.